CoCrMo Dental Metal Cobalt Chromium Molybdenum Alloy Bar Rod Superalloy Stellite Medical
Product Details:
| Place of Origin: | CHINA |
| Brand Name: | ZHEMU |
| Certification: | ISO |
| Model Number: | Standard and Customization |
Payment & Shipping Terms:
| Minimum Order Quantity: | Not limited |
|---|---|
| Price: | As Per Quotation |
| Packaging Details: | Plywood Box |
| Delivery Time: | 25-35 days |
| Payment Terms: | T/T |
| Supply Ability: | 5000kg per Week |
|
Detail Information |
|||
| NAME: | CoCrMo Dental Metal Cobalt Chrome Molybdenum Alloy Bar/rod Superalloy Stellite For Medical Use | Material: | Cocrmo |
|---|---|---|---|
| Chemical Composition: | Cocrmo | Shape: | Rod |
| Color: | Silver/Gray | Density: | 19.2g/cm3 |
| Highlight: | molybdenum alloy rod,cobalt chromium molybdenum alloy,Superalloy Stellite |
||
Product Description
CoCrMo Dental Metal Cobalt Chrome molybdenum alloy bar/rod Superalloy Stellite for medical use
|
Material:
|
Cobalt chromium molybdenum CoCrMo Dental alloy for medical use
|
|
Shape:
|
Bar
|
|
Color:
|
Natural metal color
|
|
Size:
|
Accept customized
|
|
Specification:
|
as agreement
|
|
Advantage:
|
Strong corrosion resistance, High-Temperature Resistance
|
|
MOQ
|
1KG
|
Stellite/Stellite alloy is a kind of cobalt-based superalloy. Unlike many other materials that sacrifice toughness to improve wear resistance and corrosion resistance, Stellite series alloys have both, with excellent wear resistance, heat resistance Hardness, corrosion resistance and excellent mechanical properties are the materials of choice for many harsh and severe wear applications.
Extrusion die is to put the metal blank into the die cavity, under the action of strong pressure and a certain speed, force the metal out of the die cavity, so as to obtain the product with the required shape, size and certain mechanical properties. Therefore, the extrusion process uses a mold to control the flow of metal and transfer a large amount of metal volume to form parts
Application areas:
For the selection of materials of different grades, in general, the higher the hardness of Stellite alloy, the more brittle it is. Stellite alloys with lower hardness (such as Stellite 6, Stellite 12) are suitable for extruding larger size copper bars, profiled materials, or brass, aluminum for aviation, etc. Stellite alloys with higher hardness (such as Stellite 3, Stellite 20) are suitable for extruded copper wires, round bars, small-size copper bars, profiled materials, etc.
Compared with the cast Stellite on the market, the Stellite alloy extrusion die produced by powder metallurgy has the following advantages:
1. Small and uniform grains, no internal defects
2. Better performance, the tensile strength is 40% higher than the casting strength
3. Stable quality between batches